E-mail : service@ronsteel.comPhone : +8617773160488
Our products conform to GB, AISI, ASTM, DIN, EN, JIS standard for stainlesss steel coil, sheet and plate.
Product Name |
Nickel Alloy Inconel 625 Plate, Nickel Alloy Inconel 625 Sheet |
Equivalent Grade |
Inconel 625, UNS N06625, Alloy 625, W.Nr. 2.4856 |
Standard |
GB, AISI, ASTM, DIN, EN, JIS |
Process |
Hot Rolled, Cold Rolled, Forged |
Sizes |
Thickness:1-100mm, Width:500-2400mm, Length: Up to 9000mm |
Surface Treatment |
NO.1, 1D, 2D, 2B, NO.4, BA, HL, Mirror, Embossim, Sandblasted |
Fabricating |
Rolling, Bending, Sllitting, Decoiling, Cutting, Drilling, Punching, Beveling, Welding etc. |
Application |
Oil&Gas, Petroleum, Vessels, Ship Building, Water Treatment And Environmental Protection etc. |
Strength of Inconel 625 is derived from the stiffening effect of molybdenum and niobium on its nickel-chromium matrix, thus precipitation hardening treatments are not required, this combination of elements also is responsible for superior resistance to a wide range of corrosive environments of unusual severity as well as to high-temperature effects such as oxidation and carburization. Service temperatures range from cryogenic to 1800°F (982°C).
Single Plate Of Rolling Specification |
|||||
Thickness/Width |
1500 |
1800 |
2000 |
2200 |
2400 |
4-6mm |
√ |
√ |
- |
- |
- |
6-10mm |
√ |
√ |
√ |
√ |
√ |
11-12mm |
√ |
√ |
√ |
√ |
√ |
13-14mm |
√ |
√ |
√ |
√ |
√ |
17-25mm |
√ |
√ |
√ |
√ |
√ |
26-70mm |
√ |
√ |
√ |
√ |
√ |
71-100mm |
special |
special |
special |
special |
special |
Inconel 625:
Inconel 625 was especially developed to retain high strength at elevated temperature, it resists deformation at hot-working temperatures. If hot forming of this alloy is required, powerful equipment is necessary. When Alloy 625 is hot-formed, it should be heated in a furnace whose temperature is held at (but not above) 2150°F. To guard against duplex grain structure, the work should be given uniform reductions. Final minimum reductions of 15 to 20% for open-die work are recommended.
Inconel 625:
Inconel 625 can be cold-formed by standard processes. Increased tensile properties can be achieved by cold work for moderate temperature applications. Tensile strengths of more than 300,000 psi accompanied by good ductility have been developed in 0.010-0.020-in-diameter wire after 75-90% cold reduction.
Inconel 625:
Inconel 625 is best machined in the annealed condition. Low cutting speeds should be used and the cutting tool should be engaged at all times to minimize work-hardening. Adequate cut depth is necessary to assure avoiding contact with the previously formed work-hardened zone.
Material |
Ni |
Cr |
Fe |
Mo |
Nb |
C |
Mn |
Si |
N06625 |
58.0 min |
20.0-23.0 |
5.0 max |
8.0-10.0 |
3.15-4.15 |
0.10 max |
0.50 max |
0.50 max |
Material |
Tensile strength |
Yield strength 0,2 |
Elongation |
Hardness HB30 |
N06625 |
760 N/mm² |
345 N/mm² |
30% |
220HB |
What Industries Benefit Most From Using Inconel 625 Plates?
Answer:
Industries that benefit significantly from Inconel 625 plates include: Aerospace, Oil and Gas, Marine Engineering, Chemical Processing, Power Generation.
How Can I Ensure The Quality Of Inconel 625 Plates?
Answer:
Ensuring the quality of Inconel 625 plates involves sourcing from reputable suppliers who adhere to industry standards and quality assurance protocols. Look for certifications such as ASTM, ASME, or ISO standards that verify the material's compliance with required specifications. Conducting material tests, including chemical analysis and mechanical testing, can further ensure the plates meet performance expectations.
Are There Any Special Maintenance Requirements For Inconel 625 Plates?
Answer:
Inconel 625 plates generally require minimal maintenance due to their inherent corrosion resistance and durability. However, regular inspections are recommended to ensure that no external factors, such as accumulated debris or chemical exposure, have compromised their performance. In harsh environments, periodic cleaning with appropriate agents may be necessary to remove contaminants and maintain the alloy's effectiveness.