E-mail : service@ronsteel.comPhone : +8617773160488
Our products conform to GB, AISI, ASTM, DIN, EN, JIS standard for stainlesss steel coil, sheet and plate.
Product Name |
2205/2507 Stainless Steel Plate, 2205/2507 Stainless Steel Sheet |
Equivalent Grade |
2205: AISI 2205, UNS S32205, SAE 2205, DIN 1.4462, SUS 2205, X2CrNiMoN22-5-3 |
2507: AISI 2507, UNS S32750, SAE 2507, DIN 1.4410, SUS 2507, X2CrNiMoN25-7-4 |
|
Standard |
GB, AISI, ASTM, DIN, EN, JIS |
Process |
Hot Rolled, Cold Rolled, Forged |
Sizes |
Thickness: 0.3-200mm, Width: 10-4000mm |
Surface Treatment |
NO.1, 1D, 2D, 2B, NO.4, BA, HL, Mirror, Embossim, Sandblasted |
Fabricating |
Rolling, Bending, Sllitting, Decoiling, Cutting, Drilling, Punching, Beveling, Welding etc. |
Inspection |
SGS, TUV, BV, ABS, LR etc. |
Application |
Oil&Gas, Petroleum, Vessels, Ship Building, Water Treatment And Environmental Protection etc. |
2205/2507 stainless steel plate is one of the most widely used duplex stainless steel. It contains with chromium and nickel, making it extremely resistant to uniform corrosion by organic acids. The grade can be used in chemical processing, transport, and storage for a variety of industries.
Single Sheet Of Rolling Specification | |||||||
Thickness/Width | 1500 | 1800 | 2000 | 2200 | 2400 | 2500 | 3200 |
4-6mm | √ | √ | - | - | - | - | - |
6-10mm | √ | √ | √ | √ | √ | - | - |
11-12mm | √ | √ | √ | √ | √ | √ | √ |
13-14mm | √ | √ | √ | √ | √ | √ | √ |
17-25mm | √ | √ | √ | √ | √ | √ | √ |
26-70mm | √ | √ | √ | √ | √ | √ | √ |
71-120mm | special | special | special | special | special | special | special |
2205/2507 Stainless Steel Grade:
When hot forming is required, the workpiece should be heated uniformly and worked in the range of 1750 to 2250°F. The duplex stainless steel plate is quite soft at these temperatures and is readily formed.
2205/2507 Stainless Steel Grade:
2205/2507 duplex stainless steel plate is readily cold formed on equipment suited to working stainless steels. However, because of the high strength and rapid work hardening of the grade, forces substantially higher than those for austenitic steels are required to cold form it.
2205/2507 Stainless Steel Grade:
It possesses good weldability.
|
C |
Mn |
P |
S |
Si |
Cr |
Ni |
Mo |
N |
Cu |
2205 |
0.03 |
2.00 |
0.03 |
0.02 |
1.00 |
22.00-23.00 |
4.50-6.50 |
3.00-5.00 |
0.14-0.20 |
/ |
2507 |
0.03 |
1.20 |
0.035 |
0.02 |
0.80 |
24.00-26.00 |
6.00-8.00 |
3.00-5.00 |
0.24-0.32 |
0.50 |
|
Tensile Strength (min) |
Yield Strength (min) |
Elongation |
Hardness, max |
|||
|
ksi |
Mpa |
ksi |
Mpa |
/ |
Brinell.HBW |
Rockwell |
2205 |
95 |
655 |
65 |
450 |
25 |
293 |
31HRC |
2507 |
116 |
795 |
80 |
550 |
15 |
310 |
32HRC |
Is 2205 Expensive?
Answer:
904L is a non-stabilized austenitic stainless steel with copper, this grade can resist corrosion from many acids. The high cost of this grade of stainless steel, however, has caused many manufacturers to turn to the lower-cost duplex stainless steel 2205 as an alternative.
What Is Duplex Stainless Steel?
Answer:
Combining austenitic and ferritic stainless steels equally, duplex stainless steel contain chromium (21-27%), nickel (1.35-8% ), copper (0.05-3%), and molybdenum (0.05-5% ). The combination of elements makes duplex stainless steel stronger than either austenitic or ferritic steel by itself.
Which Industries Will Use Duplex Stainless Steel?
Answer:
Duplex stainless steel often gets used in chemical processing and in crafting storage-tanks and containers that ship chemicals.